Use of Steel Slag in Concrete in place of Fine and Coarse Aggregates 109 With replacement of with 75% slag the compressive strength goes on increasing as follow: 3Days 7Days 28Days M20 -4.32 -6.25 -5.62 M30 -5.11 -5.30 -5.86 C. Flexural Strength: From fig 5 and6 Flexural strength when compared with control mix for 28D