Efficient separation of iron elements from steel slag based on magnetic …
The experimental equipment and steps are shown in Fig. 1. 100 g of slag powder was weighed and placed in a magnesium oxide crucible.It was then placed in a muffle furnace (MoSi 2 resistance heating) at 1500 °C for 90 min, cooled to 1350 °C at a rate of 1 °C/min and held for 90 min, cooled to 1100 °C at 1 °C/min, then cooled to 800 …