Improving the Physical Properties of Sinter by usage …
HMDS slag in sinter making from 0 to 60 kg/t of sinter. From the test results it was found that 30 to 35 kg HMDS slag can ... dumped or used for ground filling after crushing. Based on the earlier trials at JSW steel making slag is being used up to 40 kg/t in COREX and 50 kg/t in blast furnace. However